{"id":10365,"date":"2026-02-27T19:23:24","date_gmt":"2026-02-27T18:23:24","guid":{"rendered":"https:\/\/broquetas.com\/?p=10365"},"modified":"2026-02-27T19:23:24","modified_gmt":"2026-02-27T18:23:24","slug":"lead-free-soldering-in-roofing-for-professional-installers","status":"publish","type":"post","link":"https:\/\/broquetas.com\/en\/lead-free-soldering-in-roofing-for-professional-installers\/","title":{"rendered":"Lead-free soldering in roofing for professional installers"},"content":{"rendered":"<p data-start=\"154\" data-end=\"447\">In roofing work, <strong data-start=\"171\" data-end=\"184\">soldering<\/strong> is one of the factors that most affects the <strong data-start=\"229\" data-end=\"262\">durability of an installation<\/strong>. Gutters, metal roofs, flashings, and water drainage systems are subjected to <strong data-start=\"341\" data-end=\"381\">thermal changes, expansion, humidity<\/strong>, and, in many cases, <strong data-start=\"403\" data-end=\"444\">very specific regulatory requirements<\/strong>.<\/p>\n<p data-start=\"449\" data-end=\"776\">For years, <strong data-start=\"460\" data-end=\"478\">lead soldering<\/strong> has been a common solution due to its <strong data-start=\"517\" data-end=\"540\">ease of application<\/strong>. However, the current context has changed. Today, in many projects, <strong data-start=\"609\" data-end=\"694\">lead-free soldering is not just an alternative\u2014it is the correct technical choice<\/strong>. Understanding <strong data-start=\"710\" data-end=\"736\">when and why to use it<\/strong> is key to avoiding problems later on.<\/p>\n<h2 data-start=\"778\" data-end=\"826\">New technical requirements in roofing work<\/h2>\n<p data-start=\"828\" data-end=\"929\">Modern roofing is <strong data-start=\"846\" data-end=\"890\">more complex than it was a few years ago<\/strong>. On-site, it is common to work with:<\/p>\n<ul data-start=\"931\" data-end=\"1151\">\n<li data-start=\"931\" data-end=\"971\">\n<p data-start=\"933\" data-end=\"971\"><strong data-start=\"933\" data-end=\"969\">Galvanized and pre-treated steel<\/strong><\/p>\n<\/li>\n<li data-start=\"972\" data-end=\"1036\">\n<p data-start=\"974\" data-end=\"1036\">Components that are <strong data-start=\"994\" data-end=\"1034\">lacquered or painted after soldering<\/strong><\/p>\n<\/li>\n<li data-start=\"1037\" data-end=\"1090\">\n<p data-start=\"1039\" data-end=\"1090\">Gutters connected to <strong data-start=\"1060\" data-end=\"1088\">water collection systems<\/strong><\/p>\n<\/li>\n<li data-start=\"1091\" data-end=\"1151\">\n<p data-start=\"1093\" data-end=\"1151\">Projects with <strong data-start=\"1107\" data-end=\"1149\">very detailed technical specifications<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"1153\" data-end=\"1361\">This requires soldering not only to <strong data-start=\"1189\" data-end=\"1210\">\u201cadhere properly\u201d<\/strong> but also to <strong data-start=\"1223\" data-end=\"1260\">maintain a stable joint over time<\/strong>, even when the piece undergoes <strong data-start=\"1292\" data-end=\"1316\">subsequent processes<\/strong> or is exposed to <strong data-start=\"1334\" data-end=\"1358\">demanding conditions<\/strong>.<\/p>\n<h2 data-start=\"1363\" data-end=\"1426\">The importance of temperature in post-soldering processes<\/h2>\n<p data-start=\"1428\" data-end=\"1543\">One of the most frequent problems in roofing arises when the soldering <strong data-start=\"1499\" data-end=\"1540\">cannot withstand subsequent processes<\/strong>.<\/p>\n<p data-start=\"1545\" data-end=\"1569\">In many installations:<\/p>\n<ul data-start=\"1571\" data-end=\"1749\">\n<li data-start=\"1571\" data-end=\"1639\">\n<p data-start=\"1573\" data-end=\"1639\">Soldered components pass through <strong data-start=\"1606\" data-end=\"1637\">powder-coating curing ovens<\/strong><\/p>\n<\/li>\n<li data-start=\"1640\" data-end=\"1749\">\n<p data-start=\"1642\" data-end=\"1749\">Temperatures in these processes can <strong data-start=\"1678\" data-end=\"1747\">exceed the stability range of some traditional lead-based solders<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"1751\" data-end=\"1862\"><strong data-start=\"1751\" data-end=\"1804\">Failure is not visible at the moment of soldering<\/strong> but appears later, when the joint <strong data-start=\"1839\" data-end=\"1859\">softens or opens<\/strong>.<\/p>\n<p data-start=\"1864\" data-end=\"2071\"><strong data-start=\"1864\" data-end=\"1885\">Lead-free solders<\/strong>, with greater <strong data-start=\"1900\" data-end=\"1921\">thermal stability<\/strong>, are designed precisely to <strong data-start=\"1949\" data-end=\"1982\">prevent these types of issues<\/strong>, which often involve <strong data-start=\"2004\" data-end=\"2036\">costly rework or replacement<\/strong> of already installed components.<\/p>\n<h2 data-start=\"2073\" data-end=\"2141\">Regulatory requirements for public roofing and gutter projects<\/h2>\n<p data-start=\"2143\" data-end=\"2313\">In public works projects, the <strong data-start=\"2173\" data-end=\"2236\">use of lead-containing materials is increasingly restricted<\/strong>. Many technical specifications <strong data-start=\"2268\" data-end=\"2310\">explicitly require lead-free materials<\/strong>.<\/p>\n<p data-start=\"2315\" data-end=\"2344\">For installers, this means:<\/p>\n<ul data-start=\"2346\" data-end=\"2551\">\n<li data-start=\"2346\" data-end=\"2396\">\n<p data-start=\"2348\" data-end=\"2396\"><strong data-start=\"2348\" data-end=\"2394\">Carefully reviewing project specifications<\/strong><\/p>\n<\/li>\n<li data-start=\"2397\" data-end=\"2479\">\n<p data-start=\"2399\" data-end=\"2479\">Using <strong data-start=\"2405\" data-end=\"2444\">lead-free solder whenever indicated<\/strong>, regardless of habitual practice<\/p>\n<\/li>\n<li data-start=\"2480\" data-end=\"2551\">\n<p data-start=\"2482\" data-end=\"2551\"><strong data-start=\"2482\" data-end=\"2549\">Avoiding issues during inspection or final certification stages<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"2553\" data-end=\"2708\">In roofing, the most closely monitored points are usually <strong data-start=\"2611\" data-end=\"2657\">gutters, downspouts, and visible flashings<\/strong>, as they are part of <strong data-start=\"2679\" data-end=\"2705\">water drainage systems<\/strong>.<\/p>\n<h2 data-start=\"2710\" data-end=\"2773\">Why many private projects no longer accept lead soldering<\/h2>\n<p data-start=\"2775\" data-end=\"2865\">Beyond regulations, <strong data-start=\"2795\" data-end=\"2862\">more private projects are imposing their own technical criteria<\/strong>.<\/p>\n<p data-start=\"2867\" data-end=\"2995\">This is common in <strong data-start=\"2885\" data-end=\"2963\">large corporations, logistics centers, environmentally certified buildings<\/strong>, and <strong data-start=\"2969\" data-end=\"2992\">high-use facilities<\/strong>.<\/p>\n<p data-start=\"2997\" data-end=\"3227\">In these cases, the decision is based not only on legality but also on <strong data-start=\"3068\" data-end=\"3142\">internal safety, sustainability, and corporate responsibility policies<\/strong>. <strong data-start=\"3144\" data-end=\"3199\">Lead-free soldering is part of the project standard<\/strong> and is rarely negotiable.<\/p>\n<h2 data-start=\"3229\" data-end=\"3278\">Installer safety and health in roofing work<\/h2>\n<p data-start=\"3280\" data-end=\"3483\">Working on roofs already involves <strong data-start=\"3314\" data-end=\"3338\">demanding conditions<\/strong>: height, heat, and awkward postures. Continuous exposure to lead adds an <strong data-start=\"3412\" data-end=\"3431\">additional risk<\/strong> that many installation companies prefer to avoid.<\/p>\n<p data-start=\"3485\" data-end=\"3511\"><strong data-start=\"3485\" data-end=\"3508\">Lead-free soldering<\/strong>:<\/p>\n<ul data-start=\"3513\" data-end=\"3682\">\n<li data-start=\"3513\" data-end=\"3557\">\n<p data-start=\"3515\" data-end=\"3557\"><strong data-start=\"3515\" data-end=\"3555\">Reduces exposure to toxic substances<\/strong><\/p>\n<\/li>\n<li data-start=\"3558\" data-end=\"3609\">\n<p data-start=\"3560\" data-end=\"3609\"><strong data-start=\"3560\" data-end=\"3607\">Facilitates compliance with safety measures<\/strong><\/p>\n<\/li>\n<li data-start=\"3610\" data-end=\"3682\">\n<p data-start=\"3612\" data-end=\"3682\"><strong data-start=\"3612\" data-end=\"3643\">Improves working conditions<\/strong> without changing soldering technique<\/p>\n<\/li>\n<\/ul>\n<p data-start=\"3684\" data-end=\"3774\">It is an <strong data-start=\"3693\" data-end=\"3723\">increasingly valued factor<\/strong> by professional installers and project managers.<\/p>\n<h2 data-start=\"3776\" data-end=\"3841\">Use of lead-free solder in gutters and rainwater collection<\/h2>\n<p data-start=\"3843\" data-end=\"3942\">On roofs where rainwater is <strong data-start=\"3871\" data-end=\"3906\">collected, channeled, or reused<\/strong>, lead becomes a <strong data-start=\"3923\" data-end=\"3939\">real problem<\/strong>.<\/p>\n<p data-start=\"3944\" data-end=\"3956\">Over time:<\/p>\n<ul data-start=\"3958\" data-end=\"4104\">\n<li data-start=\"3958\" data-end=\"3990\">\n<p data-start=\"3960\" data-end=\"3990\"><strong data-start=\"3960\" data-end=\"3978\">Lead migration<\/strong> may occur<\/p>\n<\/li>\n<li data-start=\"3991\" data-end=\"4030\">\n<p data-start=\"3993\" data-end=\"4030\"><strong data-start=\"3993\" data-end=\"4022\">Water contamination risks<\/strong> arise<\/p>\n<\/li>\n<li data-start=\"4031\" data-end=\"4104\">\n<p data-start=\"4033\" data-end=\"4104\">The installation may <strong data-start=\"4054\" data-end=\"4102\">fail to meet functional project requirements<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"4106\" data-end=\"4247\">For this reason, many <strong data-start=\"4128\" data-end=\"4185\">engineers and specifiers now require lead-free solder<\/strong> in gutters and downspouts, <strong data-start=\"4213\" data-end=\"4244\">regardless of building type<\/strong>.<\/p>\n<h2 data-start=\"4249\" data-end=\"4294\">Performance of lead-free solder on site<\/h2>\n<p data-start=\"4296\" data-end=\"4386\">A common question among installers is whether <strong data-start=\"4342\" data-end=\"4383\">lead-free solder complicates the work<\/strong>.<\/p>\n<p data-start=\"4388\" data-end=\"4402\">In practice:<\/p>\n<ul data-start=\"4404\" data-end=\"4584\">\n<li data-start=\"4404\" data-end=\"4462\">\n<p data-start=\"4406\" data-end=\"4462\">Its behavior is <strong data-start=\"4422\" data-end=\"4460\">slightly different but predictable<\/strong><\/p>\n<\/li>\n<li data-start=\"4463\" data-end=\"4526\">\n<p data-start=\"4465\" data-end=\"4526\">May require <strong data-start=\"4477\" data-end=\"4524\">minor adjustments in temperature and pacing<\/strong><\/p>\n<\/li>\n<li data-start=\"4527\" data-end=\"4584\">\n<p data-start=\"4529\" data-end=\"4584\"><strong data-start=\"4529\" data-end=\"4582\">Does not require changing the soldering technique<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"4586\" data-end=\"4800\">When an <strong data-start=\"4594\" data-end=\"4624\">alloy suitable for roofing<\/strong> is used with a <strong data-start=\"4640\" data-end=\"4659\">compatible flux<\/strong>, the result is <strong data-start=\"4675\" data-end=\"4707\">stable, strong, and reliable<\/strong>. Problems usually arise when <strong data-start=\"4737\" data-end=\"4789\">lead-free solder intended for other applications<\/strong> is used.<\/p>\n<h2 data-start=\"4802\" data-end=\"4859\">Key characteristics of lead-free solder for roofing<\/h2>\n<p data-start=\"4861\" data-end=\"4916\">Before choosing a material, ensure the solder offers:<\/p>\n<ul data-start=\"4918\" data-end=\"5113\">\n<li data-start=\"4918\" data-end=\"4954\">\n<p data-start=\"4920\" data-end=\"4954\"><strong data-start=\"4920\" data-end=\"4952\">Sufficient thermal stability<\/strong><\/p>\n<\/li>\n<li data-start=\"4955\" data-end=\"4993\">\n<p data-start=\"4957\" data-end=\"4993\"><strong data-start=\"4957\" data-end=\"4991\">Good wetting on zinc and steel<\/strong><\/p>\n<\/li>\n<li data-start=\"4994\" data-end=\"5021\">\n<p data-start=\"4996\" data-end=\"5021\"><strong data-start=\"4996\" data-end=\"5019\">Controlled residues<\/strong><\/p>\n<\/li>\n<li data-start=\"5022\" data-end=\"5062\">\n<p data-start=\"5024\" data-end=\"5062\"><strong data-start=\"5024\" data-end=\"5060\">Compatibility with the flux used<\/strong><\/p>\n<\/li>\n<li data-start=\"5063\" data-end=\"5113\">\n<p data-start=\"5065\" data-end=\"5113\"><strong data-start=\"5065\" data-end=\"5111\">Compliance with RoHS and REACH regulations<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"5115\" data-end=\"5240\">These criteria are <strong data-start=\"5134\" data-end=\"5171\">far more important than unit cost<\/strong>, especially for installations exposed to <strong data-start=\"5213\" data-end=\"5237\">demanding conditions<\/strong>.<\/p>\n<h2 data-start=\"5242\" data-end=\"5308\">The value of manufacturing and specialized technical support<\/h2>\n<p data-start=\"5310\" data-end=\"5439\">Each roofing project is <strong data-start=\"5334\" data-end=\"5347\">different<\/strong>. <strong data-start=\"5349\" data-end=\"5398\">Base materials, environment, and intended use<\/strong> directly affect soldering performance.<\/p>\n<p data-start=\"5441\" data-end=\"5584\">At <strong data-start=\"5444\" data-end=\"5457\">Broquetas<\/strong>, manufacturers since 1930 in <strong data-start=\"5487\" data-end=\"5526\">Sant Andreu de la Barca (Barcelona)<\/strong>, we work with installers and installation companies to:<\/p>\n<ul data-start=\"5586\" data-end=\"5792\">\n<li data-start=\"5586\" data-end=\"5638\">\n<p data-start=\"5588\" data-end=\"5638\"><strong data-start=\"5588\" data-end=\"5636\">Define the most suitable alloy for each case<\/strong><\/p>\n<\/li>\n<li data-start=\"5639\" data-end=\"5699\">\n<p data-start=\"5641\" data-end=\"5699\"><strong data-start=\"5641\" data-end=\"5697\">Adjust the type of flux according to the application<\/strong><\/p>\n<\/li>\n<li data-start=\"5700\" data-end=\"5752\">\n<p data-start=\"5702\" data-end=\"5752\"><strong data-start=\"5702\" data-end=\"5750\">Avoid incompatibilities before going on site<\/strong><\/p>\n<\/li>\n<li data-start=\"5753\" data-end=\"5792\">\n<p data-start=\"5755\" data-end=\"5792\"><strong data-start=\"5755\" data-end=\"5790\">Reduce rework and future claims<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"5794\" data-end=\"5906\">Having <strong data-start=\"5801\" data-end=\"5851\">specialized technical support before soldering<\/strong> often makes the difference in the <strong data-start=\"5886\" data-end=\"5903\">final outcome<\/strong>.<\/p>\n<h2 data-start=\"5908\" data-end=\"5963\">Technical conclusions for professional installers<\/h2>\n<p data-start=\"5965\" data-end=\"6140\"><strong data-start=\"5965\" data-end=\"5999\">Lead-free soldering in roofing<\/strong> is not a trend or a theoretical requirement. It is a <strong data-start=\"6053\" data-end=\"6082\">proven technical solution<\/strong> designed to meet the <strong data-start=\"6104\" data-end=\"6137\">current demands of the sector<\/strong>:<\/p>\n<ul data-start=\"6142\" data-end=\"6289\">\n<li data-start=\"6142\" data-end=\"6177\">\n<p data-start=\"6144\" data-end=\"6177\"><strong data-start=\"6144\" data-end=\"6175\">Higher thermal requirements<\/strong><\/p>\n<\/li>\n<li data-start=\"6178\" data-end=\"6219\">\n<p data-start=\"6180\" data-end=\"6219\"><strong data-start=\"6180\" data-end=\"6217\">Stricter technical specifications<\/strong><\/p>\n<\/li>\n<li data-start=\"6220\" data-end=\"6254\">\n<p data-start=\"6222\" data-end=\"6254\"><strong data-start=\"6222\" data-end=\"6252\">Improved safety conditions<\/strong><\/p>\n<\/li>\n<li data-start=\"6255\" data-end=\"6289\">\n<p data-start=\"6257\" data-end=\"6289\"><strong data-start=\"6257\" data-end=\"6287\">More durable installations<\/strong><\/p>\n<\/li>\n<\/ul>\n<p data-start=\"6291\" data-end=\"6431\"><strong data-start=\"6291\" data-end=\"6320\">Choosing the right solder<\/strong> is part of the professional installer\u2019s work and <strong data-start=\"6370\" data-end=\"6428\">directly impacts the quality of the final installation<\/strong>.<\/p>\n<p data-start=\"6433\" data-end=\"6608\">If you need to <strong data-start=\"6448\" data-end=\"6491\">validate a specific roofing application<\/strong> before starting a project, the <strong data-start=\"6523\" data-end=\"6554\">technical team at Broquetas<\/strong> can help you <strong data-start=\"6568\" data-end=\"6605\">select the most suitable solution<\/strong>.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>In roofing work, soldering is one of the factors that most affects the durability of an installation. Gutters, metal roofs, flashings, and water drainage systems are subjected to thermal changes, expansion, humidity, and, in many cases, very specific regulatory requirements. For years, lead soldering has been a common solution due to its ease of application. [&hellip;]<\/p>\n","protected":false},"author":29,"featured_media":10362,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_joinchat":[],"footnotes":""},"categories":[124],"tags":[],"class_list":["post-10365","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-news-en"],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v26.9 - https:\/\/yoast.com\/product\/yoast-seo-wordpress\/ -->\n<title>Lead-free soldering in roofing for professional installers - BROQUETAS, S.L.<\/title>\n<meta name=\"description\" content=\"In roofing work, soldering is one of the factors that most affects the durability of an installation.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/broquetas.com\/ca\/?p=10368\" \/>\n<meta property=\"og:locale\" content=\"en_US\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Lead-free soldering in roofing for professional installers - BROQUETAS, S.L.\" \/>\n<meta property=\"og:description\" content=\"In roofing work, soldering is one of the factors that most affects the durability of an installation.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/broquetas.com\/ca\/?p=10368\" \/>\n<meta property=\"og:site_name\" content=\"BROQUETAS, S.L.\" \/>\n<meta property=\"article:published_time\" content=\"2026-02-27T18:23:24+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp\" \/>\n\t<meta property=\"og:image:width\" content=\"1920\" \/>\n\t<meta property=\"og:image:height\" content=\"1080\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/webp\" \/>\n<meta name=\"author\" content=\"Equipo Broquetas\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Written by\" \/>\n\t<meta name=\"twitter:data1\" content=\"Equipo Broquetas\" \/>\n\t<meta name=\"twitter:label2\" content=\"Est. reading time\" \/>\n\t<meta name=\"twitter:data2\" content=\"4 minutes\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\/\/schema.org\",\"@graph\":[{\"@type\":\"Article\",\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368#article\",\"isPartOf\":{\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368\"},\"author\":{\"name\":\"Equipo Broquetas\",\"@id\":\"https:\/\/broquetas.com\/#\/schema\/person\/6b051f950a84ab5d6d9d516588d73916\"},\"headline\":\"Lead-free soldering in roofing for professional installers\",\"datePublished\":\"2026-02-27T18:23:24+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368\"},\"wordCount\":837,\"publisher\":{\"@id\":\"https:\/\/broquetas.com\/#organization\"},\"image\":{\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage\"},\"thumbnailUrl\":\"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp\",\"articleSection\":[\"News\"],\"inLanguage\":\"en-US\"},{\"@type\":\"WebPage\",\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368\",\"url\":\"https:\/\/broquetas.com\/ca\/?p=10368\",\"name\":\"Lead-free soldering in roofing for professional installers - BROQUETAS, S.L.\",\"isPartOf\":{\"@id\":\"https:\/\/broquetas.com\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage\"},\"image\":{\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage\"},\"thumbnailUrl\":\"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp\",\"datePublished\":\"2026-02-27T18:23:24+00:00\",\"description\":\"In roofing work, soldering is one of the factors that most affects the durability of an installation.\",\"breadcrumb\":{\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368#breadcrumb\"},\"inLanguage\":\"en-US\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\/\/broquetas.com\/ca\/?p=10368\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"en-US\",\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage\",\"url\":\"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp\",\"contentUrl\":\"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp\",\"width\":1920,\"height\":1080,\"caption\":\"Soldadura sin plomo roofing\"},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\/\/broquetas.com\/ca\/?p=10368#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"Home\",\"item\":\"https:\/\/broquetas.com\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Lead-free soldering in roofing for professional installers\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\/\/broquetas.com\/#website\",\"url\":\"https:\/\/broquetas.com\/\",\"name\":\"BROQUETAS, S.L.\",\"description\":\"\",\"publisher\":{\"@id\":\"https:\/\/broquetas.com\/#organization\"},\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\/\/broquetas.com\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"en-US\"},{\"@type\":\"Organization\",\"@id\":\"https:\/\/broquetas.com\/#organization\",\"name\":\"BROQUETAS S.L.\",\"url\":\"https:\/\/broquetas.com\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"en-US\",\"@id\":\"https:\/\/broquetas.com\/#\/schema\/logo\/image\/\",\"url\":\"https:\/\/broquetas.com\/wp-content\/uploads\/2021\/08\/logo-broquetas-dark.png\",\"contentUrl\":\"https:\/\/broquetas.com\/wp-content\/uploads\/2021\/08\/logo-broquetas-dark.png\",\"width\":262,\"height\":150,\"caption\":\"BROQUETAS S.L.\"},\"image\":{\"@id\":\"https:\/\/broquetas.com\/#\/schema\/logo\/image\/\"},\"sameAs\":[\"https:\/\/www.linkedin.com\/in\/broquetas-s-l-broquetas-99a22283\/\",\"https:\/\/www.youtube.com\/channel\/UCDYxB3N3CMqWo9DA-oyiAdg\"]},{\"@type\":\"Person\",\"@id\":\"https:\/\/broquetas.com\/#\/schema\/person\/6b051f950a84ab5d6d9d516588d73916\",\"name\":\"Equipo Broquetas\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"en-US\",\"@id\":\"https:\/\/broquetas.com\/#\/schema\/person\/image\/\",\"url\":\"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g\",\"contentUrl\":\"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g\",\"caption\":\"Equipo Broquetas\"},\"url\":\"https:\/\/broquetas.com\/en\/author\/equipo-broquetas\/\"}]}<\/script>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"Lead-free soldering in roofing for professional installers - BROQUETAS, S.L.","description":"In roofing work, soldering is one of the factors that most affects the durability of an installation.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/broquetas.com\/ca\/?p=10368","og_locale":"en_US","og_type":"article","og_title":"Lead-free soldering in roofing for professional installers - BROQUETAS, S.L.","og_description":"In roofing work, soldering is one of the factors that most affects the durability of an installation.","og_url":"https:\/\/broquetas.com\/ca\/?p=10368","og_site_name":"BROQUETAS, S.L.","article_published_time":"2026-02-27T18:23:24+00:00","og_image":[{"width":1920,"height":1080,"url":"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp","type":"image\/webp"}],"author":"Equipo Broquetas","twitter_card":"summary_large_image","twitter_misc":{"Written by":"Equipo Broquetas","Est. reading time":"4 minutes"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/broquetas.com\/ca\/?p=10368#article","isPartOf":{"@id":"https:\/\/broquetas.com\/ca\/?p=10368"},"author":{"name":"Equipo Broquetas","@id":"https:\/\/broquetas.com\/#\/schema\/person\/6b051f950a84ab5d6d9d516588d73916"},"headline":"Lead-free soldering in roofing for professional installers","datePublished":"2026-02-27T18:23:24+00:00","mainEntityOfPage":{"@id":"https:\/\/broquetas.com\/ca\/?p=10368"},"wordCount":837,"publisher":{"@id":"https:\/\/broquetas.com\/#organization"},"image":{"@id":"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage"},"thumbnailUrl":"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp","articleSection":["News"],"inLanguage":"en-US"},{"@type":"WebPage","@id":"https:\/\/broquetas.com\/ca\/?p=10368","url":"https:\/\/broquetas.com\/ca\/?p=10368","name":"Lead-free soldering in roofing for professional installers - BROQUETAS, S.L.","isPartOf":{"@id":"https:\/\/broquetas.com\/#website"},"primaryImageOfPage":{"@id":"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage"},"image":{"@id":"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage"},"thumbnailUrl":"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp","datePublished":"2026-02-27T18:23:24+00:00","description":"In roofing work, soldering is one of the factors that most affects the durability of an installation.","breadcrumb":{"@id":"https:\/\/broquetas.com\/ca\/?p=10368#breadcrumb"},"inLanguage":"en-US","potentialAction":[{"@type":"ReadAction","target":["https:\/\/broquetas.com\/ca\/?p=10368"]}]},{"@type":"ImageObject","inLanguage":"en-US","@id":"https:\/\/broquetas.com\/ca\/?p=10368#primaryimage","url":"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp","contentUrl":"https:\/\/broquetas.com\/wp-content\/uploads\/2026\/02\/soldadura-sin-plomo-roofing.webp","width":1920,"height":1080,"caption":"Soldadura sin plomo roofing"},{"@type":"BreadcrumbList","@id":"https:\/\/broquetas.com\/ca\/?p=10368#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https:\/\/broquetas.com\/"},{"@type":"ListItem","position":2,"name":"Lead-free soldering in roofing for professional installers"}]},{"@type":"WebSite","@id":"https:\/\/broquetas.com\/#website","url":"https:\/\/broquetas.com\/","name":"BROQUETAS, S.L.","description":"","publisher":{"@id":"https:\/\/broquetas.com\/#organization"},"potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/broquetas.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"en-US"},{"@type":"Organization","@id":"https:\/\/broquetas.com\/#organization","name":"BROQUETAS S.L.","url":"https:\/\/broquetas.com\/","logo":{"@type":"ImageObject","inLanguage":"en-US","@id":"https:\/\/broquetas.com\/#\/schema\/logo\/image\/","url":"https:\/\/broquetas.com\/wp-content\/uploads\/2021\/08\/logo-broquetas-dark.png","contentUrl":"https:\/\/broquetas.com\/wp-content\/uploads\/2021\/08\/logo-broquetas-dark.png","width":262,"height":150,"caption":"BROQUETAS S.L."},"image":{"@id":"https:\/\/broquetas.com\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.linkedin.com\/in\/broquetas-s-l-broquetas-99a22283\/","https:\/\/www.youtube.com\/channel\/UCDYxB3N3CMqWo9DA-oyiAdg"]},{"@type":"Person","@id":"https:\/\/broquetas.com\/#\/schema\/person\/6b051f950a84ab5d6d9d516588d73916","name":"Equipo Broquetas","image":{"@type":"ImageObject","inLanguage":"en-US","@id":"https:\/\/broquetas.com\/#\/schema\/person\/image\/","url":"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g","contentUrl":"https:\/\/secure.gravatar.com\/avatar\/a76b37caac985cbb28e6dc967b1624a0dfb1eb33adaa9dd522bb7fe6d339b859?s=96&d=mm&r=g","caption":"Equipo Broquetas"},"url":"https:\/\/broquetas.com\/en\/author\/equipo-broquetas\/"}]}},"_links":{"self":[{"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/posts\/10365","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/users\/29"}],"replies":[{"embeddable":true,"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/comments?post=10365"}],"version-history":[{"count":1,"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/posts\/10365\/revisions"}],"predecessor-version":[{"id":10366,"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/posts\/10365\/revisions\/10366"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/media\/10362"}],"wp:attachment":[{"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/media?parent=10365"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/categories?post=10365"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/broquetas.com\/en\/wp-json\/wp\/v2\/tags?post=10365"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}